Microhardness test | Nanoindentation
- Equipment: Fischer H100 XYp
- Messmethode: Instrumented Indentation Test
- Standard: DIN EN ISO 14577
- Load range: 0,4 mN to 1000 mN (Microhardness, Nanoindentation, Nanohardness)
- Protection against environmental influences by an active anti-vibration table and an enclosed measurement chamber (necessary in nanoscale)
Hardness measurement of
- Thin and thick films (e.g. PVD, CVD, electroplated, lacquer etc.)
- Bulk materials
- Polished sections of thin films
- Parts
- etc.